Application cases

Acoustics and dynamic pressure

Weld monitoring: porosity and wire-stuck detection

Listen to the process right next to the arc to detect porosity and filler-wire sticking live, where an electrical sensor is drowned in the arc's interference.

Backed by measurements See the results

Discuss your application

Weld monitoring: porosity and wire-stuck detection

The need

In TIG welding, porosity or a filler wire sticking to the weld pool degrades the weld. Detecting them during welding, rather than at final inspection, makes it possible to stop or correct the process at the right time.

Each defect has an acoustic signature: the outgassing of a pore, the mechanical impulse of a sticking wire. The sensor still has to sit close to the arc and listen without interference.

Why conventional sensors fall short

  • The arc and its power cables radiate strong electromagnetic interference that mixes with the signal of a microphone or a piezoelectric sensor.
  • Reference acoustic-emission sensors require careful grounding and shielding.
  • Wire sticking does not always show on the arc current.
  • Close to the workpiece, heat and spatter limit conventional sensors.

What fiber optics brings

  • Passive sensing head with no electronics: no interference picked up, even next to the arc
  • Installed without shielding, directly on the workpiece or in contact with the cooling water bath
  • Full galvanic isolation between the welding cell and the acquisition system
  • Bandwidth of several hundred kHz for detailed spectral analysis
Why fiber optics?

Measurement results

We installed Alpheus and Evotis sensors on a robotic TIG-orbital welding cell, alongside a Vallen AMSY5 reference acoustic-emission chain, on tube-to-plate and multi-pass welds in aluminum and steel.

Porosity: on a multi-pass weld, layers were deliberately produced with and without porosity. The porous layers show higher background activity between arc strike and arc off, and their spectrum changes repeatably. The main line near 100 Hz is the process fundamental; the secondary lines between 300 Hz and 3 kHz discriminate sound layers from porous ones. On the full recording, the moments of strong high-frequency activity match the porous area found when inspecting the bead.

Wire stuck: in orbital tube welding with an internal water bath, wire sticking produces a short, strong burst, clearly separated from the arc noise. The sensor, in direct contact with the water bath, detects it with no extra protection.

Robotic TIG-orbital welding cell (ABB arm) with its acquisition chain.
Robotic TIG-orbital welding cell (ABB arm) with its acquisition chain.
The Vallen AMSY5 reference acoustic-emission chain and the Phonoptics conditioner record simultaneously. Zoom: the fiber optic sensor mounted on the workpiece, with no electrical connection.
The Vallen AMSY5 reference acoustic-emission chain and the Phonoptics conditioner record simultaneously. Zoom: the fiber optic sensor mounted on the workpiece, with no electrical connection.
Sound layer (28, blue) and porous layers (29 red, 30 yellow): time signals and spectra. The lines between 300 Hz and 3 kHz discriminate the porous layers.
Sound layer (28, blue) and porous layers (29 red, 30 yellow): time signals and spectra. The lines between 300 Hz and 3 kHz discriminate the porous layers.
Spectrogram of the whole weld run and photo of the beads: the arrows mark the high-frequency activity matching the porous area circled on the bottom bead.
Spectrogram of the whole weld run and photo of the beads: the arrows mark the high-frequency activity matching the porous area circled on the bottom bead.
Wire sticking in orbital welding with an internal water bath: a clear burst on the signal and spectral broadening (arrows). Right: the sensor in direct contact with the bath.
Wire sticking in orbital welding with an internal water bath: a clear burst on the signal and spectral broadening (arrows). Right: the sensor in direct contact with the bath.

Phonoptics R&D campaign on a robotic TIG-orbital welding cell, from the Evotis and Alpheus white paper.

Implementation

  1. The sensor is mounted on the workpiece, on the fixture or in contact with the cooling water bath, as close as possible to the weld.
  2. The fiber carries the signal to the conditioner outside the cell: MiniMyotis for a fixed measurement chain, Myotis for field tests.
  3. The BNC analog output connects to your acquisition system, alongside your other sensors.
  4. We choose the membrane for the useful frequency band and the pressure seen by the sensor.

Products used

An application close to yours?

Tell us about your installation, the temperature range and what you need to detect: we will propose the right sensor, membrane and conditioner.

Discuss your application

Other application cases

All application cases